10Cr9Mo1VNbN seamless steel pipe

10Cr9Mo1VNbN seamless steel pipe

Standard: GB/T5310

When the temperature below 620 ℃, stress of 10Cr9Mo1VNbN pipe is higher than the austenitic stainless steel.

E-mail: [email protected]

Chat OnlineLeave a message

A213 T91    A335 P91
10Cr9Mo1VNbN seamless steel pipe features: 
10Cr9Mo1VNbN pipe not only has high oxidation resistance and high temperature steam corrosion performance, but also has good impact toughness and high stability and lasting plasticity and thermal strength. When the temperature below 620 ℃,  stress of 10Cr9Mo1VNbN pipe is higher than the austenitic stainless steel.
Chemical component

Grade

C

Si

Mn

Cr

Mo

V

Ni

Alt

Nb

N

P

S

10Cr9Mo1VNbN

0.08-0.12

0.20-0.50

0.30-0.60

8.00-9.50

0.85-1.05

0.18-0.25

0.40

0.020

0.06-0.10

0.030-0.070

0.020

0.010

Mechanical property

Grade

Tensile Strength

Yield strength

Elongation (%)

Impact Energy (J)

Hardness

Mpa

Mpa

Longitudinal

Transverse

Longitudinal

Transverse

HBW

HV

HRC

10Cr9Mo1VNbN

585

415

20

16

40

27

250

260

25

Available size: OD 51-508mm     THk: 4-100mm     L: 5000-12000mm   
Delivery state: Normalizing+Tempering/ Quenching+Tempering
Application: 
10Cr9Mo1VNbN seamless pipe can be used as subcritical, supercritical boiler wall temperature ≤ 625 ℃ high temperature superheater, reheater steel pipe, and wall temperature ≤ 600 ℃ high temperature header and steam pipes, and also as a nuclear power heat exchanger and oil cracking furnace tube.
 
 