What are the welding methods of alloy steel pipe
In order to prevent welding deformation of alloy steel pipe, each column joint is symmetrically welded by two people, and the welding direction is from the middle to both sides. After welding one to three layers, reverse gouging should be carried out. After the application of carbon arc gouging, the welding machinery and equipment should be polished, and the welding surface should be nitrided to show the metal texture and prevent cracks from surface carbonization. The outer hole should be welded once, and the other inner holes should be welded once.
In the electric welding of alloy steel pipe, it is necessary to start welding from the arc striking plate and finish welding on the arc striking plate. Cut off, polish and clean after welding.
The alloy steel pipe should be tempered within 12 hours after welding. If the alloy steel pipe cannot be quenched and tempered immediately, the suggestions of heat preservation and slow cooling should be taken. When tempering, the temperature of two thermal resistances should be measured, and the thermal resistances should be welded on both sides of the weld.
-
DIN17175 10CrMo910 steel pipe
-
DIN17175 15Mo3 steel pipe featur
-
What is DIN17175 St45.8 steel pi
-
DIN17175 St35.8 steel pipe chara
-
What is API 5L PSL2 X70MO pipeli
-
API 5L PSL2 X65M pipeline steel
-
API 5L PSL2 X60MO pipeline steel
-
API 5L PSL2 X56MO pipeline pipe
-
API 5L PSL2 X52MO pipeline steel
-
API 5L PSL2 X46M concepts and fe
Product
Contact
- Henan BEBON Iron&Steel co., ltd.
- 0086-371-86151827
- 0086-371-86011881
- [email protected]
- Online Consultation
-
1358 tons 35CrMo pipes for Tanza
We exported 1358 tons 35CrMo seamless pipe to Tanzania in Ap ...
-
1200 tons SA204Gr.B Seamless pip
NNPC has long-term cooperation with SINOPEC---China Petroleu ...
-
A106M GRB PIPE FOR BIR SEBA Fiel
The Pipelines and Products Marketing Company (PPMC) by oil m ...